Fields of application
DG 4726-0008 can be used as a universal basecoat beneath Hesse PU multi-coat lacquers and top coats to build up open-pored surface finishes on all interior fittings in living areas. {Reference (Object) not found: tb4996505973384}
Technical specifications
Appearance |
colourless
|
Density series kg/l |
0.935
|
Flow time (+/- 15 %) |
40 s / DIN 53211 - 4 mm
|
Form of delivery |
fluid
|
Non-volatile content series % |
23
|
Proportion of renewable raw materials % |
4.5
|
VOC EU % |
76.720001 %
|
Number of coats (max) |
3
|
Amount per layer (minimum) |
100 g/m²
|
Amount per layer (max) |
130 g/m²
|
Total application volume |
300 g/m²
|
Mixing ratio (by volume) |
10 : 1 PU Hardener DR 4070
|
Mixing ratio (gravimetric) |
100 : 10 PU Hardener DR 4070
|
Information on use
Usage time |
8 h / 20 °C
|
Pot life |
8 h / 20 °C
|
Drying |
2 h / 20 °C
|
Stackable after |
> 16 h / 20 °C
|
Complete drying |
7 d / 20 °C
|
Surface preparation |
Clean, dry wood, dependent upon wood type and method of application.
|
Substrate sanding grits from-to |
150 - 180
|
Lacquer sanding (grit) from - to |
320 - 400
|
Finishing |
Can be coated with matching Hesse top coats after adequate drying and careful sanding. (e.g. with the ranges DE 4259x(gloss level), DE 4503x(gloss level), DE 4232x(gloss level)-0003, DE 4215x(gloss level)-0002)
|
Yield per coat |
7 - 9 m²/l
The spreading rate is heavily dependent on the type of application. The specifications relate to a liter of ready-for-use product, if necessary including hardener and thinner.
|
Storage temperature |
16 - 25 °C
|
Working temperature |
20 °C
|
Processing instructions |
It is possible to apply one to three-coats at 100 - 130 g/m² on suitable substrates. The maximum application amount in wet film totals 300 g/m². Forced drying is possible at up to 50 °C.
|
Particular instructions |
Hardening with DR 4070 at a mixing ratio (by volume) 5 : 1 enables it to be used on bleached surfaces.
|
General instructions on workmanship |
PU lacquers should not be applied and dried at material and room-temperatures below 18 °C and 40 % RH. Ideal values are: 20 - 25 °C, 50 - 65 % RH. Deviations will result in drying or hardening errors. In order to avoid adhesion problems, please sand the PU lacquered surfaces before applying fresh lacquer and apply lacquer to the sanded surfaces as soon as possible. Old lacquer and hardener mixtures affect the surface quality (adhesion/resistance). Freshly bleached substrates must undergo intermediate drying for at least 48 h at 20 °C before coating with suitable PU lacquers. If stored correctly (at least 20 °C room temperature), the final hardness of the coating is achieved after a week. Please apply a test coat under real conditions!
|
The coating process and the precise treatment parameters are adapted in each case to the respective application and drying conditions and can be found in the customer-specific process descriptions (surface techniques).
Material Safety Data Sheets
Contact
Our technical information is continually adapted to keep up to date with the latest technology and statutory regulations. The latest version is always
available online at www.hesse-lignal.de or talk to your local account manager. This information is for advice and is based on the best knowledge
available and careful research in line with the current state of the art. This information cannot be held as legally binding. We also refer you to our
terms and conditions of business. Safety data sheet is provided in accordance with EC regulation no. 1907/2006.